Dear All

I need to install line plates (2 mm thick) inside a pulp storage tower. The designer recommend the electrode ESAB OK 63.34 (vertical down welding).
My concern is the contractor has no remote control to perform it and as far as I know, after we burn 50% of the electrode rod the deposition is very hard to handle without the control.
Could you please advise me. I have the following activites in my mind.

1) Buy remote controls
2) Weld as it is (consumable wasting)
3) Change the electrodes and weld vertical up pulsing

Thanks in advance

Gustavo