The flux core welding calculator for steel 1/8 inch, .035 (0.9mm) wire, 175 - 185 IPM, 140 -155 Amperage, 14 - 15 Volts.
I can figure out the IPM for 1 - 10 wire speed.
How does 14 - 15 Volts = 1 - 10 on the Volt on the MIG 140?