    When I got started I did all cut with 4.5 Angle Grinder. Cuts were not always 90 or 45 degree a had to finish with hand file fix. I got this cheap angle grinder holder which allowed me to cut 1 angle iron 90-degree square with less filing. When I got my Porter Cable 14 chop saw I put the angle grinder holder aside till now. I attached a 3/16 plate with two 1 angle iron pieces welded to it at 90 degree so that the cutting blade cut it in half giving me two 45 degrees angle. Making it easy to cut off the angle iron corner so I can weld 90 degree corner angle with the angle iron.

    Name:  IMG_0217.jpg
Views: 202
Size:  40.9 KB Name:  IMG_0218.jpg
Views: 139
Size:  40.2 KB

    Name:  IMG_0220.jpg
Views: 179
Size:  69.2 KB Name:  Angle Iron Cut.png
Views: 133
Size:  1.4 KB
    Equipment owned: Longevity MIG 140
    Miller Classic Series Auto Darkening Helmet and MIG (lined) gloves
    Porter Cable 14 Chop Saw & 3 Angle (4.5) Grinders
    Black & Decker 10 Table Saw- Hand Drill Hand Jig Saw 7.5 Circular Saw
    Central Machinery Bench Drill Press
    Wen 6 Bench Grinder
    Support our Troops

  2. #2
    Pretty slick.
    Units owned Longevity PROmts 200

    Force Cut LP80 plasma cutter
    Longevity auto dark welding helmet

    Atlas 10x36" lathe
    Craftsman 5HP 30 Gal compressor
    Home made CNC router/plasma/hot wire foam cutting, 3D printing table powered by Longevity Force Cut LP80
    Home built aluminum foundry, HF 4x6 bandsaw

  3. #3
    Junior Member
    Join Date
    Jul 2017
    Location
    Southern New Mexico
    Posts
    8
    I discovered a flaw in my design that could me to get hurt. I need make the distance between the cutting blade and the angle iron brace greater because the piece that gets cut off could get jammed between the blade and the angle iron brace and at the high speed that the blade is turning who know what could happen. I also adapted the jig to fit my 14 Porter Cable abrasive chop saw because the small chop saw will not cut 2 angle iron. See pictures of jig attached to 14 chop saw.
    Attachment 11053 Name:  IMG_0225.jpg
Views: 125
Size:  38.9 KB
    Attached Images Attached Images  
    Last edited by Rctodd952; 07-27-2017 at 04:24 PM. Reason: Pictures to large
    Equipment owned: Longevity MIG 140
    Miller Classic Series Auto Darkening Helmet and MIG (lined) gloves
    Porter Cable 14 Chop Saw & 3 Angle (4.5) Grinders
    Black & Decker 10 Table Saw- Hand Drill Hand Jig Saw 7.5 Circular Saw
    Central Machinery Bench Drill Press
    Wen 6 Bench Grinder
    Support our Troops

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •