    I just recently bought a longevity 200SX I've been practicing both on steel and aluminum bead on plate which is been going relatively well every time I try to weld an inside corner joint or lap joint I just booger the hell out of it wines up making a big molton mess can anyone give me any advice or video out with this problem

  2. #2
    you need to control more of your heat input and watch your puddle
    Longevity ForceCut 42i
    Longevity 205p Mig W/spool gun
    HTP 201 Tig
    HTP 2400 Mig
    and more tools then my Wife wished I had

  3. #3
    Senior Member
    Join Date
    Dec 2010
    Location
    Andover, Ohio
    Posts
    308
    Welding Tips and Tricks. com

  4. #4
    General you will need slightly more amperage and more tungsten stick out

  5. #5
    just keep a eye on your puddle .
    Last edited by Gadget; 10-17-2017 at 09:32 AM. Reason: unauthorized link

  6. #6
    try tweaking the wire feed speed