    migweld 200s gun question

    ok I have looked on the web site and I can't find the ceramic piece that goes into the gun just before the copper tip. mine started cracking and falling apart the second time I used the machine. My machine is less than 30 days old is this something that happens a lot that I should have spares?

  2. #2
    Senior Member
    Join Date
    Dec 2010
    Location
    Andover, Ohio
    Posts
    311
    Welcome to the forum Sean.