    I see that this model is no longer made. I bought this in February of 2011. It is used several times a week and has performed flawlessly. This thing has been dropped, knocked over, and all around generally abused.

    It does get blown out after each use though.

    I would like to find another copy of the owners manual since I cannot find mine after moving.

  2. #2
    Hi Mad Machinist and welcome to the forum. Here's a link to the manual for the LP-60D.
    Dan
    http://forum.longevity-inc.com/attac...4&d=1257826622
    Units owned Longevity PROmts 200

    Force Cut LP80 plasma cutter
    Longevity auto dark welding helmet

    Atlas 10x36" lathe
    Craftsman 5HP 30 Gal compressor
    Home made CNC router/plasma/hot wire foam cutting, 3D printing table powered by Longevity Force Cut LP80
    Home built aluminum foundry, HF 4x6 bandsaw

  3. #3
    Thank you. The manual says this one will sever 1.5" on 220V I finally got it on 220V so we will see how it does on some 1". Have a wood chipper project coming up.

  4. #4
    Quote Originally Posted by Mad Machinist View Post
    Thank you. The manual says this one will sever 1.5" on 220V I finally got it on 220V so we will see how it does on some 1". Have a wood chipper project coming up.
    Sounds like fun, I hope you'll be able to post some photos of the work.
    Units owned Longevity PROmts 200

    Force Cut LP80 plasma cutter
    Longevity auto dark welding helmet

    Atlas 10x36" lathe
    Craftsman 5HP 30 Gal compressor
    Home made CNC router/plasma/hot wire foam cutting, 3D printing table powered by Longevity Force Cut LP80
    Home built aluminum foundry, HF 4x6 bandsaw

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •