    Trying to figure out what the problem may be with my Clarke EN130. When I squeeze the gun without striking an arc the wire comes out of the gun quite smooth but when welding it seems to be inconsistent I made sure the spool tension was not too tight. I have a new Miller on the way but just did not want to write off the Clark because it's a cheap welder and an off brand. It did work pretty good at one time not too long ago. With that said I don't just like throwing parts at it. Could the PCB be bad? Any help would be greatly appreciated.

    if this topic is covered in another thread feel free to post link
    Last edited by Merklife; 02-21-2016 at 08:29 AM.

  2. #2
    check your contact tip is in good condition, nozzle cleared, and whip is straight, wire feed set or setting set correct
    Longevity ForceCut 42i
    Longevity 205p Mig W/spool gun
    HTP 201 Tig
    HTP 2400 Mig
    and more tools then my Wife wished I had

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •