    hydraulic pipe expander project

    Made my own version of hydraulic pipe expander for about $80
    Attached Images Attached Images              
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  2. #2
    Senior Member
    Join Date
    Dec 2010
    Location
    Andover, Ohio
    Posts
    308
    Nice build.

  3. #3
    Senior Member Sling's Avatar
    Join Date
    Jan 2015
    Location
    Wash DC metro
    Posts
    110
    I like it- and I understand what it does, but I don't recognize all those parts. Do you mind explaining a touch further? "Pump the handle on the hydraulic, and that turns the [fill in blank] which causes the [fill in blank] to expand.

    What's the max wall thickness it will expand?
    Victor o/a
    accumulating tools as projects demand

  4. #4
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Quote Originally Posted by Sling View Post
    I like it- and I understand what it does, but I don't recognize all those parts. Do you mind explaining a touch further? "Pump the handle on the hydraulic, and that turns the [fill in blank] which causes the [fill in blank] to expand.

    What's the max wall thickness it will expand?

    I used the harbor freight hydraulic punch set and theor exhaust expander then machined an arbor to adapt the hydraulic part to the expander

    Not sure on Wall thickness I will have to do some testing
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •