    Stickweld 140 Update

    Thought I would give an update on the little Stickweld 140.

    It has become my favorite stick machine, due mostly to its portability and digital readout.
    I usually have it running off of an extension cord to the dryer outlet in the garage, or my 4000 watt continuous generator.
    When on the 110 side o the generator, I stick with 3/32 rods, and when on the dryer outlet, 1/8 6011 and 3/32 7018, because I don't have to change the amperage.

    I am in the process of welding out this pit made from a pair of large propane tanks.
    Attached Images Attached Images  

  2. #2
    You roasting elephants? That's a seriously big pit. Looks like a fun project. You should put this in the projects section as an entry in the latest contest.
    Units owned Longevity PROmts 200

    Force Cut LP80 plasma cutter
    Longevity auto dark welding helmet

    Atlas 10x36" lathe
    Craftsman 5HP 30 Gal compressor
    Home made CNC router/plasma/hot wire foam cutting, 3D printing table powered by Longevity Force Cut LP80
    Home built aluminum foundry, HF 4x6 bandsaw