    I haven't been here for awhile and it looks like the forum has been gutted. There used to be a tech section with this thread but unfortunately it's now gone. There was a spec for adjusting the HF Arc starter inside the machine. Every once in awhile I clean mine and reset it, but what is the distance supposed to be between the two tabs?

    It's an older 250PI vintage 2010.


    Moe Colontonio

  2. #2
    Nevermind I found it. For the archives, the correct distance between the HF Arc Start Points is .030 - .035. I find it helpful to clean these off with a little 200 grit emery cloth every once in awhile.