    3" aluminized steel showed up to build a custom exhaust
    Attached Images Attached Images  
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  2. #12
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Cut at 210 ipm and turned out pretty good imo
    Attached Images Attached Images  
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  3. #13
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Spending some quality time porting the head
    Attached Images Attached Images  
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  4. #14
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Getting closer
    Attached Images Attached Images  
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  5. #15
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Modified manifold
    Attached Images Attached Images  
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  6. #16
    Senior Member scooba's Avatar
    Join Date
    Oct 2014
    Location
    south jersey
    Posts
    127
    Just looked at the mandral bend website. That stuff is cheap and i think i might have seen some of there stuff at a local swap meet. How was the shipping on your box of bends price wise.
    Millermatic 212
    Lincoln 110 flux core

  7. #17
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Shipping was 30 for the box of bends and 2 4' sections
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  8. #18
    Senior Member scooba's Avatar
    Join Date
    Oct 2014
    Location
    south jersey
    Posts
    127
    Thibk i found my new exhaust supplier. Lol
    Millermatic 212
    Lincoln 110 flux core

  9. #19
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Very cool scooba
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  10. #20
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Injectors showed up
    Attached Images Attached Images  
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •