    Stickweld 140

    Can anyone tell me what your experience is when using the Stickweld 140, pertaining to what is the thickest metal I can actually expect to weld while set at it highest settings? Thanks

  2. #2
    Authorized Longevity Dealer blueriver's Avatar
    Join Date
    May 2014
    Location
    SE Oklahoma
    Posts
    239
    I've got one and love the little machine. I use mine in my mfg'ing of grapples and accumulators. Most of that is 3/8" thick material and find with a 7018 I need to set in the 116-121 amp range ... the thickest I have to weld on them is the hydraulic cylinder mounts which are 3/4" material standing upright on 3/8" plate with 1/4" by 3" 45degree brace brackets as reinforcement ... it handles that just fine as well .... thats a 4" weld

    I use very little 6011 rods ... but when I do they seem to burn hot on this machine. Its a great little welder.
    Last edited by blueriver; 01-13-2015 at 06:12 AM.
    5x10 CNC table
    Stickweld 140
    Forcecut 80i
    Forcecut 62i
    Tractors, Trucks,
    Trailers, Farm
    Equipment!!

  3. #3
    Blueriver, My machine also appears to be burning the 6011 rod a little too hot also. How about the size rod that you use? I bought 7018 and 6011 both in the 3/32" size. I had some 6010 in 1/8" size and I cant even get a spark while plugged in to 110 house outlet and set to 140 amps. Do I need to be plugged in to 220 to strike and burn any 1/8" rod?

  4. #4
    Authorized Longevity Dealer blueriver's Avatar
    Join Date
    May 2014
    Location
    SE Oklahoma
    Posts
    239
    Quote Originally Posted by HFDARFF View Post
    Blueriver, My machine also appears to be burning the 6011 rod a little too hot also. How about the size rod that you use? I bought 7018 and 6011 both in the 3/32" size. I had some 6010 in 1/8" size and I cant even get a spark while plugged in to 110 house outlet and set to 140 amps. Do I need to be plugged in to 220 to strike and burn any 1/8" rod?
    I've run 220V all the time ... I'll plug it in tomorrow on 110 and fire away and see what results I get ... as they say ... Stand by!!!
    5x10 CNC table
    Stickweld 140
    Forcecut 80i
    Forcecut 62i
    Tractors, Trucks,
    Trailers, Farm
    Equipment!!

  5. #5
    I was able to get my Stickweld 140 to a friend's house and plug it into a 220 outlet. It lights off the 1/8" rod just fine and burns through them without a hiccup. I guess you must have 220v to even think about running 1/8 rods so it's time to install a 220v outlet in my garage.

  6. #6
    Authorized Longevity Dealer blueriver's Avatar
    Join Date
    May 2014
    Location
    SE Oklahoma
    Posts
    239
    Quote Originally Posted by HFDARFF View Post
    I was able to get my Stickweld 140 to a friend's house and plug it into a 220 outlet. It lights off the 1/8" rod just fine and burns through them without a hiccup. I guess you must have 220v to even think about running 1/8 rods so it's time to install a 220v outlet in my garage.
    I'm so sorry ... I just didn't get to it ... I still want to see what it does ... I'll try to remember to do that today!
    5x10 CNC table
    Stickweld 140
    Forcecut 80i
    Forcecut 62i
    Tractors, Trucks,
    Trailers, Farm
    Equipment!!

  7. #7
    Senior Member Sling's Avatar
    Join Date
    Jan 2015
    Location
    Wash DC metro
    Posts
    110
    Quote Originally Posted by HFDARFF View Post
    time to install a 220v outlet in my garage.
    If you have an electric dryer you might wire up an extension cord with a dryer plug on one end and a receptacle that fits the 140 plug (looks like a NEMA 6-50, but I can't tell for sure). I run my extension cord out a window and weld outside.
    Victor o/a
    accumulating tools as projects demand

  8. #8
    Authorized Longevity Dealer blueriver's Avatar
    Join Date
    May 2014
    Location
    SE Oklahoma
    Posts
    239
    Well I finally got to it ... on 110 the 7018 both the 3/32 and 1/8 I couldn't tell a difference in 110V to the 220V arc starting ... however on the 6011 1/8 (only had 1/8") took some scratching to get it ... then there was a little "stick" but a few attempts and I was doing okay ... I prefer the 220v but I could put up with the 110
    5x10 CNC table
    Stickweld 140
    Forcecut 80i
    Forcecut 62i
    Tractors, Trucks,
    Trailers, Farm
    Equipment!!

  9. #9
    Authorized Longevity Dealer blueriver's Avatar
    Join Date
    May 2014
    Location
    SE Oklahoma
    Posts
    239
    I did more on the 110 ... it is doable ... I did this because a potential customer asked ... its really a good weld ... Needs a dedicated circuit or it will pop the breaker
    5x10 CNC table
    Stickweld 140
    Forcecut 80i
    Forcecut 62i
    Tractors, Trucks,
    Trailers, Farm
    Equipment!!

  10. #10

    Stickweld 140

    Quote Originally Posted by blueriver View Post
    I did more on the 110 ... it is doable ... I did this because a potential customer asked ... its really a good weld ... Needs a dedicated circuit or it will pop the breaker
    Here is a pic I took with my camera. the pic is not too good, but it may give an idea of what THE MACHINE RUNS LIKE ON 120V.
    As mentioned, a dedicated 20 amp circuit is really required for the machine to run properly.
    Most of what you see was done with my PowerPartner 4000 generator, except the 1/8 6011.

    This started out as a fillet weld, a 1/8 piece to a 1/4" piece.
    I started with 3/32 6013 at 65 amps, which was too cold I increased the amps with each pass, to 85 or 90 amps, at which time, I started getting more spatter.

    The last bead, on top, is a 1/8 6011 at I think 75 or 80. It was done the following day on household 20 amp circuit (not a dedicated circuit).
    I had to run it cold, because at 100 amps, it popped the breaker.

    3/32 6011 runs well on 120v, laying in there very nicely.