    Welding table overhaul

    I decided to to a over haul on my welding table, right now it is 3'x6' and I'm gonna make it 3'x4' to gain some space back in the garage one section is 3/8" oiled and pickled plate the other part is a t-slot table from a big knee mill, I am going to incorporate the receiver style accessory ports and possibly cut slots in the plate like the jmr table. All I have done at this point is rough out the legs










    To make the legs I cut apart a 4x4 left over from a project
    Attached Images Attached Images        
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  2. #2
    Authorized Longevity Dealer blueriver's Avatar
    Join Date
    May 2014
    Location
    SE Oklahoma
    Posts
    239
    Ah yes ... when I made mine I just made the top out of anything I had ... No pattern but wanted a slated top to clamp material down ... some are 2" apart and some 10" apart,, works well!!!

    Keep us up to date on the project.
    5x10 CNC table
    Stickweld 140
    Forcecut 80i
    Forcecut 62i
    Tractors, Trucks,
    Trailers, Farm
    Equipment!!

  3. #3
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Leveling feet for the table legs
    Attached Images Attached Images      
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  4. #4
    Senior Member scooba's Avatar
    Join Date
    Oct 2014
    Location
    south jersey
    Posts
    127
    Nice feet were they something you bought or made?
    Millermatic 212
    Lincoln 110 flux core

  5. #5
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Quote Originally Posted by scooba View Post
    Nice feet were they something you bought or made?
    I have had these for a while, can't really remember where they came from
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  6. #6
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Started building the frame out of 2x3 11ga tube
    Attached Images Attached Images        
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  7. #7
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Got the legs attached
    Attached Images Attached Images  
    Last edited by dzljon; 01-02-2015 at 11:08 PM.
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  8. #8
    Senior Member scooba's Avatar
    Join Date
    Oct 2014
    Location
    south jersey
    Posts
    127
    Looks like it's coming out good
    Millermatic 212
    Lincoln 110 flux core

  9. #9
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    Cut the caster plates from 1/4"
    Attached Images Attached Images      
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

  10. #10
    Authorized Longevity Dealer dzljon's Avatar
    Join Date
    Nov 2014
    Location
    Jacksonville Florida
    Posts
    576
    A freakin bomb went off
    Attached Images Attached Images  
    Machines:


    LONGEVITY 250EX 25' WELDCRAFT CS310 TORCH
    LONGEVITY FORCECUT 62i

    TORCHMATE w/ FLASH CUT CNC controls

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •