    MIG wire for stainless?

    Is there a brand or make of flux core wire for stainless steel or for welding stainless to mild steels?

    Thanks,

    DocChuck

  2. #2
    yes its 309 and you can get it in hard wire or flux core
    http://www.weldingwarehouseinc.com/ is a good source
    Ahp 200x tig acdc
    forcecut 42i
    Miller xmt350
    Lincoln LN-25
    Victor oxy/acetylene/
    Bunch of tools of the trade to much to list
    http://instagram.com/weldor_wes/

  3. #3

  4. #4
    Blue Demon 308LFC-ox is good