    AC? What. I hate stick welding in AC. Use DC.
    And yes it matters.
    Do you want to stick weld in DCEN or DCEP. Mostly it's DCEN, but it depends on the stick electrode. Look at the box and it will tell you what the recommendation is.
    Torchmate 2x2 CNC
    Longevity 200ex
    Longevity Forcecut 42i
    Thermal Arc 186

  2. #12
    Senior Member Cope's Avatar
    Join Date
    Nov 2012
    Location
    Houston, Texas
    Posts
    373
    Quote Originally Posted by Gamble View Post
    AC? What. I hate stick welding in AC. Use DC.
    And yes it matters.
    Do you want to stick weld in DCEN or DCEP. Mostly it's DCEN, but it depends on the stick electrode. Look at the box and it will tell you what the recommendation is.
    Actually, most DC is Reverse Polarity (DCEP). Actually, I made a mistake in my post, but it was too late to correct it. I usually use electrode + for AC on this machine. Since AC alternates, it may not make a difference.

    As far as AC welding, for many years it was the industry standard. I imagine there are many more AC machines in home and auto shops than AC/DC or DC only.
    4T or not 4T, that is the question.

    Miller Model 88 250 amp AC, Miller MM210, Hobart HH187, Longevity Force Cut 42i, Longevity Tigweld 200EX