    Stick Welding Steel to Cast Iron + Clamp Mini-Project

    Goodmorning everyone!!


    So, this is my latest mini-project:





    Recently, I wished I had a way to tack things to the "inside" of my table... Too far from the edges to conventionally clamp them... And this is what I came up with...


    I bought a BESSEY 8" C clamp from the local lowes, spark tested it to determine it was malleable iron, and then cut if off and simply 7018'd it to a couple scraps of mild steel plate, which I can tack anywhere I need to...


    Anyway, the clamp welded very well... It was my first time welding malleable cast iron, and first time welding dissimilar metals...


    And I got another tool for the shop... I'm pretty happy with how it came out


    Just thought I'd share... I'm probably not the first one to come up with this idea... Hope you guys enjoy the video, and have an awesome weekend everyone



  2. #2
    I like it! I guess I will be building me a couple of them. Way to go ChuckE
    Steve
    Miller Dialarc 250
    Lincoln Ranger250
    Longevity TigWeld 200DX

  3. #3
    Good idea, I'll probably wind up with a couple of them too.
    Units owned Longevity PROmts 200

    Force Cut LP80 plasma cutter
    Longevity auto dark welding helmet

    Atlas 10x36" lathe
    Craftsman 5HP 30 Gal compressor
    Home made CNC router/plasma/hot wire foam cutting, 3D printing table powered by Longevity Force Cut LP80
    Home built aluminum foundry, HF 4x6 bandsaw

  4. #4
    Great idea. You've got another person who's going to make one.
    Is it OK to want to break something just so that you can weld it back together?

  5. #5
    Senior Member roberts56's Avatar
    Join Date
    Oct 2012
    Location
    Metro Manila, Philippines
    Posts
    266
    hahaha, cool idea Lanse !! I guess I'll be making too a couple of those clamps,

    Thanks for sharing your cool ideas here man !
    HiTronic 300 amp DC Inverter IGBT Welder
    YAMATO 300 amp AC Stick Welder
    YAMATO 200 amp DC Inverter IGBT Welder
    DeWALT Cut Off Saw
    HOBART and ESAB Welding Helmets
    Assorted angle grinders : DeWALT, MAKITA, BLACK&DECKER, BOSCH, MILWAUKEE
    Assorted clamps, vises, and PPEs


    -----------------------------------
    Dreaming of a MIG, a TIG welder and a PLASMA Cutter.

  6. #6
    Haha, glad y'all like this little project!! It was fun to make... Thanks for watching

  7. #7
    Member
    Join Date
    Mar 2014
    Location
    Coimbatore,Tamil Nadu
    Posts
    90
    Quote Originally Posted by ChuckE2009 View Post
    Goodmorning everyone!!


    So, this is my latest mini-project:





    Recently, I wished I had a way to tack things to the "inside" of my table... Too far from the edges to conventionally clamp them... And this is what I came up with...


    I bought a BESSEY 8" C clamp from the local lowes, spark tested it to determine it was malleable iron, and then cut if off and simply 7018'd it to a couple scraps of mild steel plate, which I can tack anywhere I need to...


    Anyway, the clamp welded very well... It was my first time welding malleable cast iron, and first time welding dissimilar metals...


    And I got another tool for the shop... I'm pretty happy with how it came out


    Just thought I'd share... I'm probably not the first one to come up with this idea... Hope you guys enjoy the video, and have an awesome weekend everyone


    i really like this video awesome and helpful

  8. #8
    Member
    Join Date
    Mar 2014
    Location
    Coimbatore,Tamil Nadu
    Posts
    90
    Quote Originally Posted by ChuckE2009 View Post
    Goodmorning everyone!!


    So, this is my latest mini-project:





    Recently, I wished I had a way to tack things to the "inside" of my table... Too far from the edges to conventionally clamp them... And this is what I came up with...


    I bought a BESSEY 8" C clamp from the local lowes, spark tested it to determine it was malleable iron, and then cut if off and simply 7018'd it to a couple scraps of mild steel plate, which I can tack anywhere I need to...


    Anyway, the clamp welded very well... It was my first time welding malleable cast iron, and first time welding dissimilar metals...


    And I got another tool for the shop... I'm pretty happy with how it came out


    Just thought I'd share... I'm probably not the first one to come up with this idea... Hope you guys enjoy the video, and have an awesome weekend everyone


    video is really nice and helpful because it shows the desired steps for welding steel to cast iron