    Goodmorning ladies and gentlemen!!


    So, I'd had a number of requests to try welding some aluminum with those specialty electrodes you can buy, and to see how well they work, exactly...


    One afternoon on my to school, I stopped by the local Tractor Supply and bought a box of Hobart's finest, 1/8" 4043 aluminum electrodes... I got some scraps of 1/4" plate, and some thinner stuff, and got to work.








    How'd it go, you ask? Not too well, honestly... At first I couldn't get these things to run at all, and through the course of the night had virtually every stick welding problem known to man, and several known to monkey.


    They were hard to strike...


    They were hard to keep lit...


    There was slag, epic slag.


    It was hard to remove.


    It got trapped in the bead.


    It snuffed out the arc.


    My main problem was with cold lap, lack of fusion, and tie-in. These electrodes burn FAST, not fast as in 7024 or flux-core fast, fast as in they pretty much just vaporize. You have to move along the joint very fast, much too fast to get adequate tie-in. Sooo... "Why don't you just slow down?" One might ask...


    Because if you do, the metal just piles up on top of itself and is still too cold. The slag piles up too, and gets into the bead and eventually just snuffs out the arc. One can't simply "slow down" like you could on steel...


    I'm no good with these things... And honestly, I don't feel too bad about it. I know it was my first time stick welding aluminum and all, but I dont think these particular electrodes will work out well under the best of circumstances.


    Atleast for me, 99% of aluminum repairs I've seen involve a nice spool gun, or a tig machine, and I now know why that is. A bunch of people in the comments section of this video claimed to try stick welding aluminum, with the same results I had. One guy said he could get good results with the process, but the particular electrodes I used, were among the worst he'd ever bought.


    I know, I know, blame the tool, right?


    Either way, Im sure someone out there, at some point in time has gotten beautiful welds with aluminum stick electrodes, but what was I hoping for?


    I was hoping that this was something that a guy with a little previous stick welding experience could try his hand at and weld up his broken aluminum lawn mower deck. Or fix the crack on the bellhousing of his project truck. Annnnnd, its not that easy, as it turns out.


    I hope you guys enjoy the video, and yes, I do expect to get somewhat flamed for it. For the record, I'm NOT presenting this as a How-To or anything like that, its just "I got this... This is how it worked for me".


    Like I said, I hope you guys enjoy it. Despite my "less than perfect" results, it was honestly pretty fun to make






  2. #2
    Moderator KHK's Avatar
    Join Date
    Oct 2008
    Location
    Chicago suburbs
    Posts
    2,702
    Nice try!! I am glad that I have a TIG machine.
    keith
    The older the Boys, the more expensive the TOYS
    Previously Owned equipment;
    lot's
    Current equipment;
    3HP Speedair air compressor, Wilton drill press, Craftsman 10x36 lathe, 10 ton hydrolic press, Portaband band saw, OA torch, Small home brew CNC machine, powered by my 200PI
    2 Longevity autodarking helmets
    160d MIG
    WeldAll 200PI

  3. #3
    Member
    Join Date
    Mar 2014
    Location
    Coimbatore,Tamil Nadu
    Posts
    90
    Name:  92e4601e.jpg
Views: 3697
Size:  44.8 KB This is for my first aluminum stick welding..

  4. #4
    Never tried stick welding aluminum. We used to try and oxy-acc. it with anything but the best results. Sort of looked like a bulls a$$ sewn up with a grape vine.
    Steve
    Miller Dialarc 250
    Lincoln Ranger250
    Longevity TigWeld 200DX

  5. #5
    What do ya'll think about those "Alumi Weld" brazing rods?
    re: https://www.youtube.com/watch?v=y-iw...layer_embedded

  6. #6
    Hi, image is not showing!

  7. #7
    This is a 5 year old post by the user with links to external photos. The external photos have most likely been deleted or moved at the external site. No way for us to correct the links.
    Units owned Longevity PROmts 200

    Force Cut LP80 plasma cutter
    Longevity auto dark welding helmet

    Atlas 10x36" lathe
    Craftsman 5HP 30 Gal compressor
    Home made CNC router/plasma/hot wire foam cutting, 3D printing table powered by Longevity Force Cut LP80
    Home built aluminum foundry, HF 4x6 bandsaw

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •