  1. #1

    Clampable weld square

    This is an project that when made well will speed up squaring. I drew it out of 1/4x1 crs bar stock you can use just about any bar stock. Square or round material can be clamped inside or out. I suggest you v out the areas to be welded so you can grind smooth at completion. Don't put welds on the inside of the 10" long pieces so you can clamp any shape without interference.
    Attached Images Attached Images  
    Last edited by Gadget; 08-21-2011 at 07:56 PM. Reason: Made sticky
    Started welding 1991
    Equipment owned: Millermatic Vintage, vertical mill, lathe, drill presses, lots of handheld tools power and otherwise. Pretty complete woodworking shop.

    LONGEVITY try before you buy units:
    TigWeld 200DX
    Arcmate 160D
    StickWeld 140
    Forcecut 40D

  2. #2
    Nice Jon, thanks for sharing. Looks like I'll have another project.
    It was nice to meet you today, I had fun.
    Dan
    Last edited by Gadget; 08-21-2011 at 08:06 PM.
    Units owned Longevity PROmts 200

    Force Cut LP80 plasma cutter
    Longevity auto dark welding helmet

    Atlas 10x36" lathe
    Craftsman 5HP 30 Gal compressor
    Home made CNC router/plasma/hot wire foam cutting, 3D printing table powered by Longevity Force Cut LP80
    Home built aluminum foundry, HF 4x6 bandsaw

  3. #3
    Moderator KHK's Avatar
    Join Date
    Oct 2008
    Location
    Chicago suburbs
    Posts
    2,702
    Looks great, good idea!!
    keith
    The older the Boys, the more expensive the TOYS
    Previously Owned equipment;
    lot's
    Current equipment;
    3HP Speedair air compressor, Wilton drill press, Craftsman 10x36 lathe, 10 ton hydrolic press, Portaband band saw, OA torch, Small home brew CNC machine, powered by my 200PI
    2 Longevity autodarking helmets
    160d MIG
    WeldAll 200PI

  4. #4

    actual photos

    I took some hasty pics today in case anyone is interested.
    Attached Images Attached Images      
    Started welding 1991
    Equipment owned: Millermatic Vintage, vertical mill, lathe, drill presses, lots of handheld tools power and otherwise. Pretty complete woodworking shop.

    LONGEVITY try before you buy units:
    TigWeld 200DX
    Arcmate 160D
    StickWeld 140
    Forcecut 40D

  5. #5
    That helps a lot, thanks Jon.
    Units owned Longevity PROmts 200

    Force Cut LP80 plasma cutter
    Longevity auto dark welding helmet

    Atlas 10x36" lathe
    Craftsman 5HP 30 Gal compressor
    Home made CNC router/plasma/hot wire foam cutting, 3D printing table powered by Longevity Force Cut LP80
    Home built aluminum foundry, HF 4x6 bandsaw

  6. #6
    Senior Member gilly's Avatar
    Join Date
    Jul 2010
    Location
    Perdido Bch. Al.
    Posts
    870
    I got to get me one of these.I might make about 3 of them.Small to large.Nice idea.
    Guy

    Miller Syncrowave 250 DX
    Millermatic Challenger Mig
    Century 230/140 amp AC/DC Stick
    DeVilbiss 6Hp 60Gal.
    HF Horizontal/Vertical Bandsaw
    HF 6in. Belt 9in. Disc Sander
    HF pipe bender
    HF tubing roller
    Springfield machine tool co. 14X40 lathe

  7. #7
    Moderator KHK's Avatar
    Join Date
    Oct 2008
    Location
    Chicago suburbs
    Posts
    2,702
    I keep adding things to ny bucket list!!! That's one draw back of the forum.
    keith
    The older the Boys, the more expensive the TOYS
    Previously Owned equipment;
    lot's
    Current equipment;
    3HP Speedair air compressor, Wilton drill press, Craftsman 10x36 lathe, 10 ton hydrolic press, Portaband band saw, OA torch, Small home brew CNC machine, powered by my 200PI
    2 Longevity autodarking helmets
    160d MIG
    WeldAll 200PI

  8. #8
    Senior Member arandall's Avatar
    Join Date
    Dec 2008
    Location
    Saskatoon, Saskatchewan, Canada
    Posts
    1,682
    Great idea SAS. It's on my to-do list now too.
    Cheers,
    Art R.

    Longevity LS200-PI multi-purpose cutter/welder,
    Miller 180 Auto-Set MIG,
    Custom 5hp compressor,

  9. #9
    Senior Member Nicholas's Avatar
    Join Date
    Sep 2011
    Location
    Nevada Sandhill
    Posts
    264
    I got to make me a couple of these. When I was building my tig cart bottle rack I taped framing squares to the pipe to hold it square. Not the ideal way. these would have made that job a breeze. Thanks for sharing.
    Longevity Force Cut LP-50D Plasma Cutter
    Lincoln SP170T Mig Welder
    Miller 330 A/B/SP Tig Welder
    Miller Two Fifty Twin AC/DC Stick Welder
    Oxy/Acetylene Rig
    Arcair gouging torch

  10. #10
    Slick. Dead easy to check the tool for square with a decent measure. Well played, sir. ^_^
    Full hand tool assortment, collecting sheet metal hammers/dollies, more time than money.

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •