    Here is a good video explaining why you get a taper on one side of the cut when plasma cutting. Keep in mind this is an Australian company. Being from Australia I think the direction needed is reversed from the northern hemisphere so you would go opposite what they say in the video. Still, it gives a good explanation of why it makes a difference.



    Another great video explaining the different types of dross and how to correct for them.



    A summary of cut height and pierce height



    Gasses



    Cutting holes



    Torch



    Pierce Height



    Lead ins



    Consumables



    CNC Stepper or server



    The Arc



    Trailing Arc



    Basic principles



    Cut Height



    Cutting corners (CNC)

    Last edited by Gadget; 12-10-2010 at 07:38 PM.
    Units owned Longevity PROmts 200

    Force Cut LP80 plasma cutter
    Longevity auto dark welding helmet

    Atlas 10x36" lathe
    Craftsman 5HP 30 Gal compressor
    Home made CNC router/plasma/hot wire foam cutting, 3D printing table powered by Longevity Force Cut LP80
    Home built aluminum foundry, HF 4x6 bandsaw

  2. #2
    Senior Member samsberr's Avatar
    Join Date
    Nov 2010
    Location
    Pendleton, OR
    Posts
    348
    Good stuff ...

    Thanks for the contribution.
    Longevity Arcmate 160
    Longevity 50i
    Longevity TigWeld 200 DX
    Longevity Water Cooler
    Torchmate 2x2
    Custom Water Table

    HF 4X6 Bandsaw
    Custom Built 16" Chop saw
    Grizzly 14" band saw
    Delta 6" vert. belt sander
    Victor O/A
    Craftsman 5hp, 30gal
    Delta Drill Press

  3. #3
    Moderator KHK's Avatar
    Join Date
    Oct 2008
    Location
    Chicago suburbs
    Posts
    2,702
    Good Info!!
    keith
    The older the Boys, the more expensive the TOYS
    Previously Owned equipment;
    lot's
    Current equipment;
    3HP Speedair air compressor, Wilton drill press, Craftsman 10x36 lathe, 10 ton hydrolic press, Portaband band saw, OA torch, Small home brew CNC machine, powered by my 200PI
    2 Longevity autodarking helmets
    160d MIG
    WeldAll 200PI

  4. #4
    Nice videos. Thanks
    I can't finish a project before I start a new one...an addiction to say the least

    Currently own: Hobart Handler 140
    Looking to purchase Longevity MIG and TIG after I get back from this deployment

  5. #5
    Thanks Gadget! Don't know how I missed this, but I just found it.
    Just Sensible Concepts
    *Longevity Weldall 160PI (technically it's not mine but it is on MY inventory for my shop at work)
    Lincoln Weldanpower 200
    Lincoln Pro Mig 180
    Lincoln AC225

  6. #6

    Coriolis...no....swirl ring yes

    [QUOTE=Gadget;21394]Here is a good video explaining why you get a taper on one side of the cut when plasma cutting. Keep in mind this is an Australian company. Being from Australia I think the direction needed is reversed from the northern hemisphere so you would go opposite what they say in the video. Still, it gives a good explanation of why it makes a difference.

    Gadget these are truly excellent vids! But.....I doubted the Coriolis effect caused the swirl to be CW in Down-under, but it was a great beer drinking thought. So I tried my cutter, sure enough he was correct, even in direction. Rather than immediately think the earth had reversed axis I took apart my torch, and what did I find??? The swirl ring, and depending on how you put it in, the swirl can be CW or CCW See attached picture and look at the port, you can see that flipped one way it directs the air CW, the other way, CCW, the ring is symmetrical, so it dont care, only the air cares.
    cheers, and thanx for the vid links they were great!
    cm2

    Name:  IMG_0137.jpg
Views: 1261
Size:  37.0 KB

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •