Aluminum wire is becoming popular again to run to panel because of copper prices. you need a bigger size and connection need a anti-oxidant on connection like Noalox.

Aluminum Wire amp rate
#8 30 amps
#6 40 amps
#4 55 amps
#2 75 amps
#1 85 amps
1/0 100 amps
2/0 115 amps
3/0 130 amps
4/0 150 amps
Hi and welcome to the forum. We like pictures here so be sure to include some showing your work. Be sure to post a bit about yourself in the introduce yourself section so we can get to know you. Also, keep an eye out for the next contest here. The odds of winning a great new Longevity machine are very good.