    3,227

    They basically told me to buy a new one.

    They basically told me to buy a new one.
  2. Replies
    2
    Views
    3,227

    Cutmaster 81 issue

    Iím not sure if this is where I should be in this section but here we go. I have a thermal dynamics cutmaster 81. It has never had a problem. Today I turned it on, but no air or arc was coming from...