    http://www.usaweld.com/Parts-for-HTP-MicroCut-600-...

    http://www.usaweld.com/Parts-for-HTP-MicroCut-600-Plasma-Cutter-Torch-p/mc25600-parts.htm?1=1&CartID=0
    Swirl ring part 62058

    Electrode is part 60003

    And cutting tips depend on how many amps...
  2. Replies
    4
    Views
    2,039

    What are your skills experience

    What are your skills experience
  3. Replies
    5
    Views
    6,309

    http://www.northerntool.com/shop/tools/product_580...

    http://www.northerntool.com/shop/tools/product_580421_580421?cm_mmc=Google-pla&utm_source=Google_PLA&utm_medium=Welding%20>%20Welding%20Accessories&utm_campaign=ReelWorks&utm_content=159188&ci_src=175...
  4. Replies
    30
    Views
    40,186

    Soo are these available yet

    Soo are these available yet
  5. Replies
    5
    Views
    2,414

    Co2 ,will meet most of your needs on that unit

    Co2 ,will meet most of your needs on that unit
  6. Replies
    11
    Views
    7,267

    I could never get the spool gun to work on 1\8th...

    I could never get the spool gun to work on 1\8th aluminium wouldn't get Penetration just sat on top my Lincoln 210 had no issues with the longevity spool Gun hooked up to it
    Works fine with steel...
  7. Replies
    5
    Views
    3,436

    Call and ask for Jesse at longevity

    Call and ask for Jesse at longevity
  8. Replies
    9
    Views
    3,114

    Yup tabs most metal suppliers carry them

    Yup tabs most metal suppliers carry them
  9. Replies
    26
    Views
    7,049

    Using a simple volt meter from the work lead to...

    Using a simple volt meter from the work lead to gun will tell you if its DC output or ac if its like the hf unit its ac output
  10. This ever sell

    This ever sell
  11. Replies
    21
    Views
    13,181

    Htp usaweld stocks them

    Htp usaweld stocks them
  12. Replies
    21
    Views
    11,400

    Those are for a 20 amp plasma there are 40 and 60...

    Those are for a 20 amp plasma there are 40 and 60 amp versions out there
  13. Replies
    18
    Views
    8,243

    ebay is a good place to find what your looking for

    ebay is a good place to find what your looking for
  14. Replies
    9
    Views
    5,789

    The 355 is a nice flowmeter same one I use

    The 355 is a nice flowmeter same one I use
  15. Replies
    14
    Views
    5,629

    dinse 50 unless they changed it the plug is for...

    dinse 50 unless they changed it
    the plug is for the spoolgun and 2t torch controls
  16. Replies
    3
    Views
    7,155

    its a really nice machine

    its a really nice machine
  17. Replies
    3
    Views
    2,439

    thin material requires thin filler if you are...

    thin material requires thin filler
    if you are practicing on stainless pipe a back purge is normally used
    for shielding on the back side you can use solar b or gas shield it
  18. Replies
    5
    Views
    2,804

    wind blocks or run flux core

    wind blocks or run flux core
  19. Replies
    4
    Views
    4,284

    for one that argon bottle is good for the tig...

    for one that argon bottle is good for the tig only unless you have a spoolgun for aluminum on the 140
    i would get co2 or c25 gas for the migs which in turn means you need more then one bottle ...
  20. Replies
    3
    Views
    6,609

    yes its 309 and you can get it in hard wire or...

    yes its 309 and you can get it in hard wire or flux core
    http://www.weldingwarehouseinc.com/ is a good source
  21. i would just pick up a 20lb co2 tank on...

    i would just pick up a 20lb co2 tank on craigslist 2 flow meters and check valves and a Y fitting do the math and get the mix you want
    interesting that you are having a problem upgrading the tank...
  22. Replies
    2
    Views
    1,976

    yup time and material is how i bid everything ...

    yup time and material is how i bid everything
    for something like that you could do a piece rate but in order to do that you would need to know what you have into in time and have it be reasonable ...
  23. i am with daniel on the 42i over the 40 d

    i am with daniel on the 42i over the 40 d
  24. Replies
    17
    Views
    7,605

    replace the liner my guess is you have a kink in...

    replace the liner my guess is you have a kink in it
    part number is on lincolns website your LWS should be able to get it or have it in stock
  25. Replies
    2
    Views
    1,963

    should be the same they have a standard they have...

    should be the same they have a standard they have to follow on the gas
Results 1 to 25 of 500
Page 1 of 20 1 2 3 4