  1. Replies
    5
    Views
    6,787

    Iv'e heard peening it is good. hit the weld with...

    Iv'e heard peening it is good. hit the weld with the ball peen while it's cooling down. like khk said. If you can anneal it that would be ideal, I don't know how to do that.

    I think drilling out...
  2. Replies
    7
    Views
    4,385

    you're welcome. I have no problem recommending it...

    you're welcome. I have no problem recommending it to anyone. I have not heard one single bad thing about it yet. I wish I would have bought a pallet load of them when they first came out and resold...
  3. Replies
    15
    Views
    11,658

    Nah. im still here guys I just had to use the...

    Nah. im still here guys I just had to use the restroom. so where were we? oh yeah. this thing is still kicking and I still love it.
  4. Replies
    7
    Views
    4,385

    I love the stickweld 140. it's my favorite...

    I love the stickweld 140. it's my favorite machine. It seems to be built really well and i tell everyone that asks to me what to get to get that baby. even if they have bigger machines or are...
  5. Honestly I use it all the time and i plug it into...

    Honestly I use it all the time and i plug it into whatever i can find. My chopsaw always trips a certin plug at my house but this machine never does. It's my favorite welding machine. I used it...
  6. Replies
    13
    Views
    4,220

    Make a video of you building it and put it on...

    Make a video of you building it and put it on youtube.
  7. Replies
    19
    Views
    4,138

    What's a borer is that like digging out a hole or...

    What's a borer is that like digging out a hole or are you not very interesting? J/k i'll google it. welcome.
  8. Replies
    5
    Views
    3,617

    I love the stickweld 140

    this machine is good at the full 140 amps and also 29 amps
    The 1st is 220 the second is 110
    I wouldn't mind getting a few of those and try selling them at this market that gets a lot of traffic...
  9. Replies
    13
    Views
    2,636

    I just tried the stickweld 140 and am really...

    I just tried the stickweld 140 and am really digging it. Im uploading a video tonight showing how bad ass it is.
    I used it @ 29 amps and 120 and 130 amps and boom it's great thats all there is to...
  10. Replies
    15
    Views
    11,658

    That ground is good enough but I like the brass...

    That ground is good enough but I like the brass ones because they don't burn up if the ground slips.
  11. Replies
    15
    Views
    11,658

    I don't have one of those tig torches but if the...

    I don't have one of those tig torches but if the stick works well than it would be good at that.
  12. Replies
    45
    Views
    10,160

    That sucks. I hope you catch them.

    That sucks. I hope you catch them.
  13. Replies
    15
    Views
    11,658

    stickweld 140. Oh yeah.

    I just received the new stickweld 140 110 220 inverter. I think my first post did not make it through. This machine looks incredible and is so small. 140amps is more than I use and it's price is...
  14. I have not had a chance to use it any more. I...

    I have not had a chance to use it any more. I need to get some aluminum. It was working very well after I got the hang of it.
  15. greetings forum. I see my old account is up again!

    I cant get on my new account but it looks like tk421 is back online! thats good. I am getting back into the welding thing after a little TCB. Im ready to make some stuff!
  16. Replies
    2
    Views
    3,372

    I sold my miller generator.

    I sold my miller generator because I never use it since I got the longevity. It was an awesome machine but too much for my needs. I am going to get a diesel generator from here in Jan for an...
  17. Replies
    72
    Views
    11,000

    I posted during the blackout. I want a hat.

    I posted during the blackout. I want a hat.
  18. Replies
    18
    Views
    3,300

    Welcome. I really like the arcmate 160d. Im...

    Welcome. I really like the arcmate 160d. Im working on some fun stuff with it. Ill post them when Im done.
  19. Replies
    15
    Views
    888

    Hey I can go to a trade show in chicago. I love...

    Hey I can go to a trade show in chicago. I love trade shows. I can use my free youtube money.
  20. Replies
    50
    Views
    50,750

    Thanks. it is really easy to plasma cut. easier...

    Thanks. it is really easy to plasma cut. easier if you use some kind of guide. it's fun.
  21. sure thing. I usually do that but I didn't fore...

    sure thing. I usually do that but I didn't fore some reason.
  22. arcmate 160d mig/stick machine. making a bottle tree.

    This is me making a bottle tree. Thats just a place to put bottles to catch evil spirits or some kinda hippy mumbo jumbo. It's not for me :roll:


    im using to stick welding function in this...
  23. Replies
    7
    Views
    5,013

    harbor freight Vs. Longevity

    Using my camera phone in the local harborfreight store. I was showing some subs the inside of the store and some machines. I threw a plug for longevity and my much loved 205i multi process machine....
  24. Here is a video of me trying out a spool gun for...

    Here is a video of me trying out a spool gun for the first time ever. I started kinda rough because I didn't open the argon but after I figured that out I stared making some decent beads. Im going to...
  25. Longevity 205i multi process stick tig plasma cutter. I love it.

    So I guess my original posts are gone here is the new Longevity 205i multiprocess machine. I completely love it. the plasma is smooth and I can cut with great control. The arc is really good on the...