any one have some basic set ups 1/16 steel/ alum.my unit should be here on the 4/9 any help or sugestions wold be help full thanks to all

EdKing
04-06-2008, 06:02 AM
I have mine set for 70 psi pressure on the air, Upslope and Downslope to 0, post flow to about 3 (helps cool of torch quicker). I am not sure on current, I haven't cut any thing that small yet, I would get a scrap piece and try different current settings until I found which works the best.

Ed

EdKing
04-06-2008, 07:49 AM
Ok, I experimented on cutting some blades for a utility knife. Set pressure to 30 psi and current to 5 amps. worked well but you have to move the torch pretty quick to keep the cut going.