DCRP means that the electrode is + and Work surface - ... I think....I always get this mixed up....Can someone help clear this up for me?? Paul

Gadget
04-09-2009, 09:51 AM
It means DC Reverse Polarity which in effect is rod positive.
Dan

MAC702
04-09-2009, 09:52 AM
Yep!

DCRP = DCEP
DCSP = DCEN