PDA
View Full Version :

CNC and 42i quality cut documentation



Gamble
02-25-2014, 11:43 AM
For those using a 42i on a CNC machine let's share our info and get a good cut quality chart going to help others.

Please list metal, thickness, amperage, speed, voltage if applicable, & torch height.


.100 aluminum 35 amps, 72ipm, approx 1/8" cut height yields me almost perfect cuts with only a few small dross spots.