110v stick on 200sx



TwistedSteel
04-17-2013, 07:01 AM
Anyone experience stick welding with a 200sx running on 110v? If so how was your experience? Mine doesn't sound right, more like it is surging rather than an even burn. This is anywhere from 90- 200 amps on 1/8" steel with 3/32" 7018

Cope
04-17-2013, 04:32 PM
I ran 110V stick on my 160SX, but I ran 6013 and 7014.