02-25-2012, 04:40 PM
Jr. College Intro to Welding SMAW. Today I worked on 2g welding in class. This my first atempt at 2g. I was moving a little fast at the end so there is some undercut there. I am improving slowly but surely. My "new to me" welder should be here next week. Then I can get some practice more than one day a week. Again any and all opinions welcomed. I have thick skin because I'm new at this and I'm 50.


http://i62.photobucket.com/albums/h112/old15bravo/d3840128.jpg