I changed the number size and reduced the overall image for this cutout. This is going to be attached to the back of my tailgate when I get it all polished up.
The CNC table now has all the kinks ironed out (so far) and it is really cool to click start and just watch it go. Tip height is .062 which seems to be optimal. Air pressure is 75psi. Amperage was at 35 which might have been a bit overkill but it doesn't flame out if the material warps and pulls away from the cut at that amperage.
The next cutout project it the POW/MIA logo. I plan on doing this over the weekend and will post it if it turns out well.