alumiweld brazing type rods for aluminum video.



Freddytk421
08-31-2010, 08:34 PM
they are supposed to be pretty strong.
CJ42scaWFnw

KHK
08-31-2010, 09:35 PM
I used something similar about 20 yrs ago, the instruction said to blacken the AL with acetylene only, then turn on the oxygen and when the black is burned off add the filler rod. It worked very well, but was very expensive!!

Another great video!!!

Gadget
09-01-2010, 06:58 AM
I've used it and still have some. Like you said in the video it takes some practice to get the feel of it but the parts I welded with it several years ago are still holding strong.

arandall
09-01-2010, 01:14 PM
Thanks Freddy. - That was interesting.

Art R.