Made these pipe extensions for the New England Cobra owners to use to pass inspection. They do two things. first they reduce the loudness as they are mufflers, and second they extend the muffler past the door openings. I donated these to be used for inspection only;)

ahack3r
08-31-2010, 07:35 PM
plus they add a little extra to the look of the Cobra ;) nice. I respect that you would donate them!

gilly
08-31-2010, 07:43 PM
Very nice set of pipes.They will definitely add to the looks of the car,while he is passing inspection.Would love to have a cobra.

KHK
08-31-2010, 09:15 PM
They look great!! What metal are they made of?

ISKI
09-01-2010, 04:56 AM
The pipes are mild steel with ceramic coat. The exensions are 304 stainless. In CT you need a bunch of changes to the original car to pass inspection. A group of us each donated one item to a kit that gets passed around. When someone needs to register a car or get inspected since they only have 1965 relectors/mirrors/wipers or they have loud exhaust and were pulled over, then they borrow the kit, bolt the stuff on, and pass;)