The ForceCut 60I looks like a fantastic unit.
Great video demo!

I can see the unit needs 208/220 input volts.
The spec's are unclear on input ampacity.
Operating Voltage:
208/220vac 50/60HZ Input Single Phase 1PH

40amp cut draws 350Amps

What is the correct input amperage requirments?

Regards,
John

LONGEVITY
09-04-2009, 05:54 PM
John,

There is an error in the specs. The 40 amp cut draws 35amps. Also, the input is 220v with a 30-50 amp breaker to be sufficient.

We test the units at a 50amp breaker 220v single phase.